1、 ENGINEERING MATERIAL SPECIFICATION Date Action Revisions 2013 12 12 N Status No replacement named L. Sinclair, NA 2007 06 21 Revised Inserted 3.0; Deleted 3.2 95 - 100% R.H. Test Method: Expose 10 in (250 mm) lengths of the bonded assembly to the environments listed above. Two hours after exposure,
2、 cut away and discard the unbonded portion of weatherstrip and windlace. Measure peel adhesion in accordance with ASTM D 413, Machine Method, except operate the testing machine at 12 in (300 mm)/min and calculate the average force required to peel the sponge rubber from the vinyl in oz/in (N/mm) of bond width.