ARMY MIL-L-15040 F (1)-1973 LABEL GARMENT (WOVEN RAYON)《衣服标签(人造丝编织)》.pdf

上传人:eveningprove235 文档编号:445510 上传时间:2018-11-16 格式:PDF 页数:4 大小:132.56KB
下载 相关 举报
ARMY MIL-L-15040 F (1)-1973 LABEL GARMENT (WOVEN RAYON)《衣服标签(人造丝编织)》.pdf_第1页
第1页 / 共4页
ARMY MIL-L-15040 F (1)-1973 LABEL GARMENT (WOVEN RAYON)《衣服标签(人造丝编织)》.pdf_第2页
第2页 / 共4页
ARMY MIL-L-15040 F (1)-1973 LABEL GARMENT (WOVEN RAYON)《衣服标签(人造丝编织)》.pdf_第3页
第3页 / 共4页
ARMY MIL-L-15040 F (1)-1973 LABEL GARMENT (WOVEN RAYON)《衣服标签(人造丝编织)》.pdf_第4页
第4页 / 共4页
亲,该文档总共4页,全部预览完了,如果喜欢就下载吧!
资源描述

1、MIL-L-15040F w-1 12 larch 1973 MILITARY SPECIFICATION LABELS, G- (WOYDl, RAYON) This Amendment forms a part of Military Specification MIL-L-l5040F, dated 26 May 1972, and is approved for use by all Departments and Agencies of the Department of Defense. PAGE 1 1.2 “1.2 Classification. Delete in its e

2、ntirety and substitute: The woven labels shall be of the following types and sizes as specified below (see 6.2). Type I - Rayon me II - Polyester Size A - 1-5/16 inches wide by 3 inches long. Size B - 3/4 inch wide by 2 inches long. Size C - 2-1/4 inches wide by 4 inches long. Size D - 2-1/4 inches

3、wide by 5 inches long. PAGE 2 3.2.1 Delete in its entirety and substitute: The type I label shall be woven of filament rayon (viscose in the denier specified.“ Add the following new paragraph: “3.2.2 Type II. The type II label shall be woven of filament polyester (PolYethYlene glycol terephthalate)

4、in the denier specified“. Delete paragraph 3.3.1 in its entirety and substitute the fo.Uowing: “3.3.1 The labels shall be woven with the following construction in a taffeta and figured weave when tested as specified in 4.2.5. . FSC 8315 i Provided by IHSNot for ResaleNo reproduction or networking pe

5、rmitted without license from IHS-,-,-MIL-L-15340F Amendment-1 Characteristic Ground warp Ground filling Figure filling Sd.vages (sizes A and B) Selvage (sizes c and D) LOO denier singles 50 denier, 2 ply or 75 denier singles o 13C denier singles 153 denier singles 100 denier singles 50 denier, 2 ply

6、 150 denier singles or or 100 denier singles 53 denier, 2 ply O 1 Texture 144 ends per inch (min) 92 picks per inch (min) 84 picks per inch (min) 84 picks per inch (min) 8 double ends each seivage 8 singles ends each selvage 12 double ens ech selvage Type II Approx. yarn size Texture 90 denier singl

7、es 144 ends or per inch 40 denier, 2 ply (min) 70 denier singles 88 picks or per inch 40 denier, 2 ply (min) i50 denier singles 88 picks per inch (min) 90 denier singles 8 double 40 denier, 2 ply selvage or . ends each 90 denier singles 12 dou6l.e 40 denier, 2 ply seivage“ i or ends ech PAGE 3 3.4,

8、last sentence. Add “Type I“, between the words, “finished“ and label“. 3.4.2 Delete in its entirety and substitute: 3.4.2 Colorfastness. The type I labels shall show colorfastness to wet It rycleaning and perspiration equal to or better than the standard sample when tested as specified in 4.2.5. The

9、 type II labels shall show colorfastness to wet drycleaning, perspiration and sublimation, equal to or better than the standard sample when tested as specified in 4.2.5. When no standard sample is available or when the standard sample is not referenced for colorfastness, the type I and II labels sha

10、ll show “good“ colorfastness to wet drycleaning, perspiration and (sublimation type II only) when testd s specified in 4.25.“ PAGE 2 of 4 Provided by IHSNot for ResaleNo reproduction or networking permitted without license from IHS-,-,-MlL-L-15040F Amendment -1 PAGE 4 Add the following paragraph: “3

11、.8 Finish. The finish OZ the label shall be equal to or better than that of the standard sample (see 6.3)“. PAGE 5 Table I add the following defect: “Finish not equal to the standard sample“. PAGE 6 Table III, under the characteristic , column. . Add “(Type I) after the word, “rayon“. Add the follow

12、ing in their respective columns: “identification of polyester (type II) 3.2.2 1600 - Under “Colorfastness to: II. Add the following in their respective columns: “Sublimation (type II only) It 3.4.2 5642 3/“ PAGE 7 Add the following footnote: Id The test shall be conducted at a temperature range of 6

13、. I 5.2.1, second sentence. Delete and substitute: %ch shipping container shall be closed in accordance with method III, waterproofed in accordance with method V, and reinforced as specified in the appendix of the container specification, I 5.2.2.1 line 3 after kith“. Insert “method III as specified

14、 in.“ 5.2.3 Delete in its entirety and substitute: “5.2.3 Level G. Labels, packaged as specified in 5.1, shall be packed in a manner to insure carrier acceptance and cgrc delivery at destination at the lowest transportation rate for such supplies. with Uniform Freight Classification Rules, or Nation

15、al Motor Freight Classification Mes, as applicable. It Containers shall be in accordance PAGE 3 of 4 Q I Y 0 Provided by IHSNot for ResaleNo reproduction or networking permitted without license from IHS-,-,-MIL-L-1504OF Amendment -1 PAGE 8 6.2 Delete Une “(b)“ and substitute the following: “(b) !Typ

16、e and size required (see 1.2 and 3.5)“. custodians: Preparing activity: Army - GL Navy - SA Air Force - 11 Army - GL Project No. 8315-0218 Review activity: Air Force - 82 User activity: Navy - MC U. S. GOVERNMENT PRINTIN0 WFICE I973 -714-543/4388 PAGE 4 of 4 t, Provided by IHSNot for ResaleNo reproduction or networking permitted without license from IHS-,-,-