1、Lessons Learned Entry: 1230Lesson Info:a71 Lesson Number: 1230a71 Lesson Date: 1999-01-21a71 Submitting Organization: JSCa71 Submitted by: Keith A Mason/ Ronald A. MontagueSubject: Welds Near Tube Bends Description of Driving Event: During dimensional inspection of orbital tube welds involving 316L

2、tubing, it was found that 8 of 8 welds failed because of weld mismatch. The weld joints were located between two bends that formed a “S“ bend. There was approximately 1 inch of straight tubing from each bend to the joint of the weld. The mismatch in this case is not to exceed 25% or 0.010 inch which

3、 ever is less.Root cause: Tube bending / shaping typically causes the tube to take an oval shape, creating matching problems during weld fitting. Engineering drawings provided insufficient length for oval / runout to occur of the shaped / bent tube prior to welding of the joint.Lesson(s) Learned: Sh

4、aping /bending of tubes must take into consideration the oval-shaped deformations that result when planning for subsequent weldsRecommendation(s): Design Engineering should use a non-welded configuration when close proximity bends are needed. Even though the orbital tube welding process requires onl

5、y 0.7 inches of straight tubing on both sides of the joint for clamping, approximately 1.5 diameters of straight tubing should be kept between a bend and a weld joint for ovality run-out. This will insure acceptable ovality that, in turn, will insure acceptable mismatch. Evidence of Recurrence Contr

6、ol Effectiveness: N/AProvided by IHSNot for ResaleNo reproduction or networking permitted without license from IHS-,-,-Documents Related to Lesson: N/AMission Directorate(s): N/AAdditional Key Phrase(s): a71 Hardwarea71 Industrial Operationsa71 NASA Standardsa71 Parts Materials & Processesa71 Safety & Mission Assurancea71 StandardAdditional Info: Approval Info: a71 Approval Date: 2002-06-27a71 Approval Name: Ronald A. Montaguea71 Approval Organization: JSCa71 Approval Phone Number: 281-483-8576Provided by IHSNot for ResaleNo reproduction or networking permitted without license from IHS-,-,-

展开阅读全文
相关资源
猜你喜欢
  • ASTM D5813-2004 Standard Specification for Cured-In-Place Thermosetting Resin Sewer Piping Systems《现场硫化固定的热固性树脂污水管系统的标准规范》.pdf ASTM D5813-2004 Standard Specification for Cured-In-Place Thermosetting Resin Sewer Piping Systems《现场硫化固定的热固性树脂污水管系统的标准规范》.pdf
  • ASTM D5813-2004(2008) 838 Standard Specification for Cured-In-Place Thermosetting Resin Sewer Piping Systems《现场硫化固定的热固性树脂污水管系统的标准规范》.pdf ASTM D5813-2004(2008) 838 Standard Specification for Cured-In-Place Thermosetting Resin Sewer Piping Systems《现场硫化固定的热固性树脂污水管系统的标准规范》.pdf
  • ASTM D5813-2004(2012) 6834 Standard Specification for Cured-In-Place Thermosetting Resin Sewer Piping Systems《现场硫化固定的热固性树脂污水管系统的标准规范》.pdf ASTM D5813-2004(2012) 6834 Standard Specification for Cured-In-Place Thermosetting Resin Sewer Piping Systems《现场硫化固定的热固性树脂污水管系统的标准规范》.pdf
  • ASTM D5814-2002 Standard Practice for Determination of Contamination in Recycled Poly(Ethylene Terephthalate) (PET) Flakes and Chips Using a Plaque Test《用蚀斑试验测定再循环聚对苯二甲酸乙酯薄膜和晶片中杂质的.pdf ASTM D5814-2002 Standard Practice for Determination of Contamination in Recycled Poly(Ethylene Terephthalate) (PET) Flakes and Chips Using a Plaque Test《用蚀斑试验测定再循环聚对苯二甲酸乙酯薄膜和晶片中杂质的.pdf
  • ASTM D5814-2010 1250 Standard Practice for Determination of Contamination in Recycled Poly(Ethylene Terephthalate) (PET) Flakes and Chips Using a Plaque Test《用蚀斑试验测定再循环聚对苯二甲酸乙酯(PET.pdf ASTM D5814-2010 1250 Standard Practice for Determination of Contamination in Recycled Poly(Ethylene Terephthalate) (PET) Flakes and Chips Using a Plaque Test《用蚀斑试验测定再循环聚对苯二甲酸乙酯(PET.pdf
  • ASTM D5814-2018 1875 Standard Practice for Determination of Contamination in Recycled Poly(Ethylene Terephthalate) (PET) Flakes and Chips Using a Plaque Test.pdf ASTM D5814-2018 1875 Standard Practice for Determination of Contamination in Recycled Poly(Ethylene Terephthalate) (PET) Flakes and Chips Using a Plaque Test.pdf
  • ASTM D5817-2003a Standard Practice for Carbon Black Pelleted&8212 Reduction Blending and Drying of Gross Samples for Testing《试验用大颗粒、准圆度混合、干燥碳黑样品的标准实施规程》.pdf ASTM D5817-2003a Standard Practice for Carbon Black Pelleted&8212 Reduction Blending and Drying of Gross Samples for Testing《试验用大颗粒、准圆度混合、干燥碳黑样品的标准实施规程》.pdf
  • ASTM D5817-2003a(2008) 866 Standard Practice for Carbon Black Pelleted - Reduction Blending and Drying of Gross Samples for Testing《碳黑 颗粒缩径和大型样品混合用标准实施规程》.pdf ASTM D5817-2003a(2008) 866 Standard Practice for Carbon Black Pelleted - Reduction Blending and Drying of Gross Samples for Testing《碳黑 颗粒缩径和大型样品混合用标准实施规程》.pdf
  • ASTM D5817-2003a(2014) 4646 Standard Practice for Carbon Black PelletedReduction Blending and Drying of Gross Samples for Testing《炭黑的标准实施规范 试验用总样品的减少 混合和干燥》.pdf ASTM D5817-2003a(2014) 4646 Standard Practice for Carbon Black PelletedReduction Blending and Drying of Gross Samples for Testing《炭黑的标准实施规范 试验用总样品的减少 混合和干燥》.pdf
  • 相关搜索

    当前位置:首页 > 标准规范 > 国际标准 > 其他

    copyright@ 2008-2019 麦多课文库(www.mydoc123.com)网站版权所有
    备案/许可证编号:苏ICP备17064731号-1