1、Designation: F1544 11 (Reapproved 2017) An American National StandardStandard Specification forDetermining the Rating Velocities of a Compound ArcheryBow1This standard is issued under the fixed designation F1544; the number immediately following the designation indicates the year oforiginal adoption

2、 or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval. Asuperscript epsilon () indicates an editorial change since the last revision or reapproval.1. Scope1.1 This specification covers the testing technique to deter-mine the rating vel

3、ocities of a compound bow.1.2 This specification will provide only a certification ofperformance, that is, the velocities at which a given bow willlaunch arrows of specified weights under standard conditions.1.3 This specification is not intended to provide any engi-neering or structural evaluation

4、of the bow that would deter-mine its fitness for the use intended, safe function, or any otherattribute except as stated.1.4 The values stated in inch-pound units are to be regardedas standard. The values given in parentheses are mathematicalconversions to SI units that are provided for information

5、onlyand are not considered standard.1.5 The following safety hazards caveat pertains only to thetest methods portion, Section 4, of this specification: Thisstandard does not purport to address all of the safety concerns,if any, associated with its use. It is the responsibility of the userof this sta

6、ndard to establish appropriate safety, health, andenvironmental practices and determine the applicability ofregulatory limitations prior to use.1.6 This international standard was developed in accor-dance with internationally recognized principles on standard-ization established in the Decision on P

7、rinciples for theDevelopment of International Standards, Guides and Recom-mendations issued by the World Trade Organization TechnicalBarriers to Trade (TBT) Committee.2. Terminology2.1 Definitions of Terms Specific to This Standard:2.1.1 archery trade association (ATA) draw length, nthedistance at t

8、he archers full draw from the string at the nockingpoint to a vertical line through the pivot point of the bow grip134 in. (+14 in., 0 in.) (44 + 6.4 0 mm).2.1.2 draw length pressure point (DLPP) draw length,nthe distance at the archers full draw from the string at thenocking point to a vertical lin

9、e through the distal or pivot pointof the bow grip.2.1.3 force-draw curvethe graph curve generated by re-cording the draw force readings of an archery bow at 1.0-in.(25.4-mm) intervals or less, from brace height through setweight and to the center of the valley (if present), in order toreveal the en

10、ergy storage characteristics of the bow.2.1.4 rating velocities, nthe initial velocity of an arrowweighing 5 grains per pound (0.073 g/N) of the bows PeakDraw Force (60.5 grains (60.03 g) on total arrow weight)(0.03 g) from a bow set at no more than 70 612 lb (311.4 N)Peak Draw Force and 30 in. (762

11、 mm) ATA actual draw length.Example: a 70-lb Peak Draw Force bow requires the use of a350 grain (22.7 g) arrow (60.5 grains (60.03 g) on total arrowweight) (0.03 g 6 0.4 N). A minimum of (5) shots for each testmust be performed. Test shot velocities will then be averagedto determine the ATA Compound

12、 Bow Rating Velocity.2.1.5 shooting machinea device, equipped with a me-chanical release, that secures a bow and releases an arrow toobtain highly repeatable shooting results for various testingpurposes.2.1.6 stored energythe energy required to draw a bowfrom brace height to full draw, usually expre

13、ssed in foot-pounds (joules).3. Significance and Use3.1 This specification will be used to determine a velocityunder standard test conditions for rating an archery bow.4. Test Methods4.1 Force Draw Data:4.1.1 For bows with adjustable draw force, adjust peak ormaximum draw force to no more than 70 6

14、0.5 lb (311.4 62.22 N). The center of the valley of the force-draw curve(lowest force) attained after having passed through the peak ormaximum draw force shall be located at 2814-in. (717.6 mm)DLPP, +14 0 in. (6 mm).4.1.2 Measure and record the draw force at 1.0-in. (25.4-mm) (or less) increments fr

15、om brace height to at least 2814-in.(717-mm) DLPP (30-in. (762-mm) ATA) draw length.1This specification is under the jurisdiction of ASTM Committee F08 on SportsEquipment, Playing Surfaces, and Facilitiesand is the direct responsibility ofSubcommittee F08.16 on Archery Products.Current edition appro

16、ved Dec. 1, 2017. Published December 2017. Originallyapproved in 1994. Last previous edition approved in 2011 as F1544 11. DOI:10.1520/F1544-11R17.This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Prin

17、ciples for theDevelopment of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.14.1.3 From the force-draw curve (obtained in 4.1.2), deter-mine the peak or maximum draw force that occurs between thebrace position of

18、 the bow and the full draw length of 2814-in.(717-mm) DLPP (30-in. (762-mm) ATA).4.2 Test Arrows:4.2.1 Select the test arrows of a shaft material, size, andsufficient spine to match the test bows Peak Draw Force anddraw length. The test arrows must also meet the 5 grain perpound (0.073 g/N) of the t

19、est bows Peak Draw Force weightrequirement (60.5 grain (0.03 g). (Refer to example shown in2.1.4).4.2.2 The arrows need not be fletched.4.3 Set up the test bow in the shooting machine.4.3.1 Mount the bow in a shooting machine with a mechani-cal release. Set the draw length at 2814-in. (717-mm) DLPP

20、(30+18, 0 in. (762 + 3.2, 0 mm) ATA).4.3.2 Set the initial chronograph gate at a distance of 36 in.(914 mm) from the pivot point of the bows handle.4.4 Shooting Test:4.4.1 Chronograph a minimum of five shots for each testarrow using the standard test arrow to obtain a satisfactoryarrow velocity aver

21、age. The average velocity is determinedfrom a minimum of five shots of the test arrow in which no testvelocity more than 2 ft/s (0.61 m/s) from any other testvelocity.4.4.2 Use an appropriate multiple gate chronograph.5. Keywords5.1 draw length; force draw curve; rating velocity; shootingmachine; st

22、ored energyASTM International takes no position respecting the validity of any patent rights asserted in connection with any item mentionedin this standard. Users of this standard are expressly advised that determination of the validity of any such patent rights, and the riskof infringement of such

23、rights, are entirely their own responsibility.This standard is subject to revision at any time by the responsible technical committee and must be reviewed every five years andif not revised, either reapproved or withdrawn. Your comments are invited either for revision of this standard or for additio

24、nal standardsand should be addressed to ASTM International Headquarters. Your comments will receive careful consideration at a meeting of theresponsible technical committee, which you may attend. If you feel that your comments have not received a fair hearing you shouldmake your views known to the A

25、STM Committee on Standards, at the address shown below.This standard is copyrighted by ASTM International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA 19428-2959,United States. Individual reprints (single or multiple copies) of this standard may be obtained by contacting ASTM at the ab

26、oveaddress or at 610-832-9585 (phone), 610-832-9555 (fax), or serviceastm.org (e-mail); or through the ASTM website(www.astm.org). Permission rights to photocopy the standard may also be secured from the Copyright Clearance Center, 222Rosewood Drive, Danvers, MA 01923, Tel: (978) 646-2600; http:/ 11 (2017)2

展开阅读全文
相关资源
猜你喜欢
相关搜索

当前位置:首页 > 标准规范 > 国际标准 > ASTM

copyright@ 2008-2019 麦多课文库(www.mydoc123.com)网站版权所有
备案/许可证编号:苏ICP备17064731号-1