1、American Welding Society 550 NW LeJeune Road Miami, Florida 33126 The purpose of an errata sheet is to notify the public that a published standard has a typographical error. Errata sheets provide a list of errors and their corrections on an AWS standard introduced during the publication stages. AWS

2、Errata Sheet The following Errata have been identified and will be incorporated into the next reprinting of this document. AWS Standard: AWS D3.6M:2010, Underwater Welding Code Page 60 - Figure 7.2, note 2bCorrect “” to “”. Page 62 - Table 7.3, replace Table 7.3 with the table shown below: Page 63Fi

3、gure 7.3, note aCorrect “” to “”. Page 63Figure 7.3, note bCorrect “” to “”. Page 72-Table 8.1, note a-Correct “First position only. Qualification for additional positions will omit groove weld tension, macroetch, and fillet weld shear strength tests.“ to “First position only. Qualification for addi

4、tional positions will omit groove weld tension, macroetch, Charpy tests, and fillet weld shear strength tests.“ Page 72-Table 8.1, note 1-Correct “WM-Weld Metal; HAZ = Heat-Affected Zone.“ to “HAZ Charpy Impact Testing is not required for qualification of wet welding procedures. WM = Weld Metal; HAZ

5、 = Heat-affected Zone.“ Page 75Figure 8.2, note 3bCorrect “” to “”. American Welding Society 550 NW LeJeune Road Miami, Florida 33126 The purpose of an errata sheet is to notify the public that a published standard has a typographical error. Errata sheets provide a list of errors and their correctio

6、ns on an AWS standard introduced during the publication stages. Page 75-Table 8.2, footnote b-Correct “See 5.11.5 and Table 8.1, Note 5.“ to “HAZ Charpy Impact Testing is not required for qualification of wet welding procedures. See 5.11.5 and Table 8.1, footnote d.“ Page 77Figure 8.3, note bCorrect “” to “”. Page 79-Table 8.3, Column heading-Correct “Fillet Weld Break (See Figure 5.9)“ to “Fillet Weld Break (See Figure 5.8)“.