DLA MIL-S-46850 D (2)-2002 STEEL BAR PLATE SHEET STRIP FORGINGS AND EXTRUSIONS 18 PERCENT NICKEL ALLOY MARAGING 200 KSI 250 KSI 300 KSI AND 350 KSI HIGH QUALITY《高质量每平方英寸200 250 300.pdf

上传人:confusegate185 文档编号:693431 上传时间:2018-12-30 格式:PDF 页数:1 大小:12.58KB
下载 相关 举报
DLA MIL-S-46850 D (2)-2002 STEEL BAR PLATE SHEET STRIP FORGINGS AND EXTRUSIONS 18 PERCENT NICKEL ALLOY MARAGING 200 KSI 250 KSI 300 KSI AND 350 KSI HIGH QUALITY《高质量每平方英寸200 250 300.pdf_第1页
第1页 / 共1页
亲,该文档总共1页,全部预览完了,如果喜欢就下载吧!
资源描述

1、MIL-S-46850D AMENDMENT 2 7 FEBRUARY 2002 SUPERSEDING AMENDMENT 1 22 November 1991 MILITARY SPECIFICATION STEEL: BAR, PLATE, SHEET, STRIP, FORGINGS, AND EXTRUSIONS, 18 PERCENT NICKEL ALLOY, MARAGING, 200 KSI, 250 KSI, 300 KSI, and 350 KSI, HIGH QUALITY This amendment forms a part of MIL-S-46850D, dat

2、ed 22 March 1991, and is approved for use by all Departments and Agencies of the Department of Defense. PAGE 4 3.2, line 3: Delete “816 + 5C” and substitute “816 + 14C”. PAGE 7 * Footnote 2 of Table II: Delete first sentence and substitute with “Critical stress intensity factor KIC = Ksi-in1/2 minim

3、um.” NOTE: The margins of this amendment are marked with asterisks to indicate where changes from the previous amendment were made. This was done as a convenience only and the government assumes no liability whatsoever for any inaccuracies in these notations. Bidders and contractors are cautioned to

4、 evaluate the requirements of this document based on the entire content irrespective of the marginal notations and relationships to the last previous amendment. Custodian: Preparing activity: Army MI DLA - IS Navy AS DLA IS (Project 9515-1153) Review activities: Army AR, MR Navy - OS AMSC N/A 1of 1 FSC 9515 DISTRIBUTION STATEMENT A. Approved for public release; distribution is unlimited. INCH POUND Provided by IHSNot for ResaleNo reproduction or networking permitted without license from IHS-,-,-

展开阅读全文
相关资源
猜你喜欢
  • ASTM C1581 C1581M-2009 Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage.pdf ASTM C1581 C1581M-2009 Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage.pdf
  • ASTM C1581 C1581M-2009a Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage《测定限制收缩下的灰浆.pdf ASTM C1581 C1581M-2009a Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage《测定限制收缩下的灰浆.pdf
  • ASTM C1581 C1581M-2016 Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage《测定限制收缩下的灰浆和.pdf ASTM C1581 C1581M-2016 Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage《测定限制收缩下的灰浆和.pdf
  • ASTM C1581 C1581M-2018 Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage《限制收缩下砂浆和混凝土.pdf ASTM C1581 C1581M-2018 Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage《限制收缩下砂浆和混凝土.pdf
  • ASTM C1581 C1581M-2018a Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage.pdf ASTM C1581 C1581M-2018a Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage.pdf
  • ASTM C1581-2004 Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage《测定限制收缩下的灰浆和混凝土断裂老化.pdf ASTM C1581-2004 Standard Test Method for Determining Age at Cracking and Induced Tensile Stress Characteristics of Mortar and Concrete under Restrained Shrinkage《测定限制收缩下的灰浆和混凝土断裂老化.pdf
  • ASTM C1582 C1582M-2004 Standard Specification for Admixtures to Inhibit Chloride-Induced Corrosion of Reinforcing Steel in Concrete《混凝土中钢筋的氯化感应腐蚀抑制用混合料的标准规范》.pdf ASTM C1582 C1582M-2004 Standard Specification for Admixtures to Inhibit Chloride-Induced Corrosion of Reinforcing Steel in Concrete《混凝土中钢筋的氯化感应腐蚀抑制用混合料的标准规范》.pdf
  • ASTM C1582 C1582M-2011 Standard Specification for Admixtures to Inhibit Chloride-Induced Corrosion of Reinforcing Steel in Concrete《用于抑制混凝土钢筋氯化物诱导腐蚀的混合物标准规范》.pdf ASTM C1582 C1582M-2011 Standard Specification for Admixtures to Inhibit Chloride-Induced Corrosion of Reinforcing Steel in Concrete《用于抑制混凝土钢筋氯化物诱导腐蚀的混合物标准规范》.pdf
  • ASTM C1582 C1582M-2011(2017)e1 Standard Specification for Admixtures to Inhibit Chloride-Induced Corrosion of Reinforcing Steel in Concrete《混凝土中钢筋氯化感应腐蚀抑制用混合料的标准规格》.pdf ASTM C1582 C1582M-2011(2017)e1 Standard Specification for Admixtures to Inhibit Chloride-Induced Corrosion of Reinforcing Steel in Concrete《混凝土中钢筋氯化感应腐蚀抑制用混合料的标准规格》.pdf