FORD FLTM BV 151-02-2001 COLD ADHESION OF SOUND DEADENER PADS (Replaces FLTM EU-BV 051-02)《隔音垫的低温粘结 替代FLTM EU-BV 051-02[替代 FORD FLTM EU-BV 051-02]》.pdf

上传人:sofeeling205 文档编号:747655 上传时间:2019-01-14 格式:PDF 页数:4 大小:45.78KB
下载 相关 举报
FORD FLTM BV 151-02-2001 COLD ADHESION OF SOUND DEADENER PADS (Replaces FLTM EU-BV 051-02)《隔音垫的低温粘结 替代FLTM EU-BV 051-02[替代 FORD FLTM EU-BV 051-02]》.pdf_第1页
第1页 / 共4页
FORD FLTM BV 151-02-2001 COLD ADHESION OF SOUND DEADENER PADS (Replaces FLTM EU-BV 051-02)《隔音垫的低温粘结 替代FLTM EU-BV 051-02[替代 FORD FLTM EU-BV 051-02]》.pdf_第2页
第2页 / 共4页
FORD FLTM BV 151-02-2001 COLD ADHESION OF SOUND DEADENER PADS (Replaces FLTM EU-BV 051-02)《隔音垫的低温粘结 替代FLTM EU-BV 051-02[替代 FORD FLTM EU-BV 051-02]》.pdf_第3页
第3页 / 共4页
FORD FLTM BV 151-02-2001 COLD ADHESION OF SOUND DEADENER PADS (Replaces FLTM EU-BV 051-02)《隔音垫的低温粘结 替代FLTM EU-BV 051-02[替代 FORD FLTM EU-BV 051-02]》.pdf_第4页
第4页 / 共4页
亲,该文档总共4页,全部预览完了,如果喜欢就下载吧!
资源描述

1、 FORD LABORATORY TEST METHOD BV 151-02 Date Action Revisions 2001 03 28 Revised Editorial no technical change A. Cockman 1990 05 24 Printed copies are uncontrolled Page 1 of 4 Copyright 2000, Ford Global Technologies, Inc. COLD ADHESION OF SOUND DEADENER PADS Application This procedure is used to de

2、termine the adhesion properties of sound deadener pads, when subjected to impact at low temperature. Apparatus Required Mechanical Convection Oven Capable of maintaining temperatures up to 250 +/- 2 C. Balance Precision +/- 0.5 g - maximum permitted load 3 kg. Cold Box Capable of maintaining a tempe

3、rature of - 40 +/- 1 C. The box must be large enough to accommodate the fixture during the slamming test. Impact Test Fixture As described and illustrated in FLTM BV 151-01. Materials Required Test Panels Preparation as in Attachment 1. Steel Body Skin Panels. Dimensions: 300 x 300 x 1.5 +/- 0.10 mm

4、 Load A. (1.0 kg) 300 x 300 x 1.5 +/- 0.10 mm Load B. (2.5 kg) Surface finish 0.9 - 1.8 micrometre C.L.A. Conditioning and Test Conditions All test values indicated herein are based on material conditioned in a controlled atmosphere of 23 +/- 2 C and 50 +/- 5 % relative humidity for not less than 24

5、 h prior to testing and tested under the same conditions unless otherwise specified. FORD LABORATORY TEST METHOD BV 151-02 Page 2 of 4 Copyright 2000, Ford Global Technologies, Inc. Procedure Method A (for Self-adhering Deadener Pads) 1. Prepare 3 test panels in accordance with FLTM BI 120-01. Deter

6、mine the weight of the individual panels (W1 ). 2. Cut 3 specimens 300 x 280 mm from the material under test. Remove the release paper from the specimens and apply to the test panels by hand pressure or roller, leaving a 20 mm strip on the top of each panel where it fits into the clamping fixture. 3

7、. Condition the test assemblies according to Attachment 1, Item 1. 4. Determine the total weight (W2 ) for each individual assembly. 5. Insert an assembly into the clamping fixture (with deadener side outermost). Remove the load (Part 5) and balance the assembly by means of the adjustable counterwei

8、ght (Part 3). 6. Attach load A or B as required, to lever (Part 4) and fix at a distance of 300 mm from the pivot center. 7. Place the assembly and impact test fixture in the Cold Box for a minimum of 3 h at a temperature of - 40 +/- 1 C, if not otherwise specified by the applicable Engineering Mate

9、rial Specification. 8. While still in the Cold Box allow the lever to fall 6 times in rapid succession from a horizontal position. 9. Remove assembly from the Cold Box and condition for 16 h at 23 +/- 2 C. 10. Remove any loose particles of test material and determine the weight (W3 ) of the assembly

10、. 11. Repeat steps 5 - 10 using the other 2 assemblies. Note: If required by the applicable Engineering Material Specification, the assemblies may be subjected to additional testing cycles according to Steps 7, 8, 9 and 10. Evaluation Calculate the percentage of material retained on each panel as fo

11、llows: Retain material (%) = W 3 W 1 x 100 W2 W1 Where: W1 = Weight of test panel. W2 = Weight of test panel plus deadener pad. W3 = Weight of test panel plus deadener pad after impact testing and removal of loose particles. FORD LABORATORY TEST METHOD BV 151-02 Page 3 of 4 Copyright 2000, Ford Glob

12、al Technologies, Inc. Method B (for Sound Deadener Pads used on E.C. Coated Surfaces) 1. Prepare 3 test panels in accordance with FLTM BI 120-01. Determine the weight of individual panels (W1 ). 2. Cut three specimens 300 x 280 mm from the material under test. Apply the specimens to the panels, leav

13、ing a 20 mm strip at the top of each panel where it fits into the clamping fixture. 3. Condition the test assembly in the oven according to Attachment 1, Item 2. The assembly must be conditioned in a horizontal position. 4. Remove the assembly from the oven, condition for 2 h at 23 +/- 2 C and deter

14、mine the total weight (W2 ) of the individual assemblies. 5. Proceed as outlined under steps 5 - 11 of Method A. Evaluation As outlined under Method A. Method C (for Sound Deadener Pads use on Oiled Surfaces) 1. Prepare 3 test panels in accordance with FLTM BZ 150-11 - normal grade. Determine the we

15、ight of the individual panels (W1 ). 2. Cut 3 specimens 300 x 280 mm from the material under test. Apply the specimens to the panels, leaving a 20 mm strip at the top of each panel where it fits into the clamping fixture. 3. Condition the test assembly in the oven according to Attachment 1, Item 3.

16、The assembly must be conditioned in a horizontal position. 4. Remove the assembly from the oven, condition for 2 h at 23 +/- 2 C and determine the total weight (W2 ) of the individual assemblies. 5. Proceed as outlined under steps 5 - 11 of Method A. Evaluation As outlined under Method A. Chemicals,

17、 materials, parts, and equipment referenced in this document must be used and handled properly. Each party is responsible for determining proper use and handling in its facilities. FORD LABORATORY TEST METHOD BV 151-02 Page 4 of 4 Copyright 2000, Ford Global Technologies, Inc. COLD ADHESION OF SOUND

18、 DEADENER PADS Attachment 1 Test Panel Test Material Preparation Conditioning Cycle Sound-deadener pads self- FLTM BI 120-01 16 h at 23 +/- 2 C (in adhering. For use on horizontal or vertical electrocoated surfaces. position) Sound-deadener pads. For FLTM BI 120-01 20 minutes at 145 +/- 2 C use on e

19、lectrocoated surfaces. air temperature - (in horizontal position). . Cool to 23 +/- 2 C Sound-deadener pads. For FLTM BZ 150-11 . 25 minutes at 165 +/-use on oiled surfaces. Normal Grade 2 C air temperature. . Cool to 23 +/- 2 C. . 25 minutes at 165 +/- 2 C air temperature. . Cool to 23 +/- 2 C. . 20 minutes at 145 +/- 2 C air temperature. . Cool to 23 +/- 2 C (in horizontal position).

展开阅读全文
相关资源
猜你喜欢
相关搜索

当前位置:首页 > 标准规范 > 国际标准 > 其他

copyright@ 2008-2019 麦多课文库(www.mydoc123.com)网站版权所有
备案/许可证编号:苏ICP备17064731号-1