1、 ENGINEERING MATERIAL SPECIFICATION Material Name Specification Number Date Action Revisions 2015 12 09 N Status No replacement D. Murtonen, NA 2003 02 27 Revised Para 3.0 inserted ; Para 3.1, 3.2, 3.3, 3.10, 3.11, 4 deleted 2000 07 31 Activated N. J. Komatsu Page 1 of 2 Copyright 2015, Ford Global
2、Technologies, Inc. FABRIC, TWILL II, PATTERN, FLAT WOVEN, WSS-M1H824-A UNLAMINATED NOT TO BE USED FOR NEW DESIGN 1. SCOPE The material defined by this specification is a woven jacquard polyester face fabric. 2. APPLICATION This specification was released originally for material used as an interior t
3、rim fabric for the 2001 Model Year. 3. REQUIREMENTS In addition to the requirements listed herein, the fabric shall meet all requirements of WSS-M8P18-A1/A2/A3/A4 as applicable. 3.0 STANDARD REQUIREMENTS FOR PRODUCTION MATERIALS Material suppliers and part producers must conform to the Companys Stan
4、dard Requirements For Production Materials (WSS-M99P1111-A). 3.4 FABRIC CONSTRUCTION 3.4.1 Fabric Count, +/- 5 % tolerance (ASTM D 3775) Warp 246 ends/10 cm Weft 132 picks/10 cm 3.4.2 Fabric Weight, min (FLTM BN 106-01) 285 - 315 g/m2 3.5 COMPOSITION (ASTM D 629) Fabric 100 % polyester ENGINEERING M
5、ATERIAL SPECIFICATION WSS-M1H824-A Page 2 of 2 Copyright 2015, Ford Global Technologies, Inc. 3.6 YARN CONSTRUCTION (ASTM D 1244) Warp 730 dtex f144 (air texturised, semi-dull) Weft 750 dtex f192 (air texturised, semi-dull) 3.7 METHOD OF DYEING Yarn dyed and spun or as approved by Materials Engineer
6、ing 3.8 FINISHED OPERATIONS As approved by Materials Engineering 3.9 FLAMMABILITY (ISO 3795/SAE J369) Burn Rate, max 100 mm/minute Note: Not required on face fabric when used as a fully bonded composite. 5. GENERAL INFORMATION The information given below is provided for clarification and assistance in meeting the requirements of this specification: 5.1 Purchase departments will ensure that both materials defined in this specification and shipped to any one assembly plant will be produced by one supplier only.