FORD FLTM AO 107-1-2001 QUANTITATIVE ANALYSIS OF TRIMETHYLAMINE.pdf

上传人:twoload295 文档编号:746815 上传时间:2019-01-14 格式:PDF 页数:5 大小:50.39KB
下载 相关 举报
FORD FLTM AO 107-1-2001 QUANTITATIVE ANALYSIS OF TRIMETHYLAMINE.pdf_第1页
第1页 / 共5页
FORD FLTM AO 107-1-2001 QUANTITATIVE ANALYSIS OF TRIMETHYLAMINE.pdf_第2页
第2页 / 共5页
FORD FLTM AO 107-1-2001 QUANTITATIVE ANALYSIS OF TRIMETHYLAMINE.pdf_第3页
第3页 / 共5页
FORD FLTM AO 107-1-2001 QUANTITATIVE ANALYSIS OF TRIMETHYLAMINE.pdf_第4页
第4页 / 共5页
FORD FLTM AO 107-1-2001 QUANTITATIVE ANALYSIS OF TRIMETHYLAMINE.pdf_第5页
第5页 / 共5页
亲,该文档总共5页,全部预览完了,如果喜欢就下载吧!
资源描述

1、 FORD LABORATORY TEST METHOD AO 107-01 Date Action Revisions 2001 01 30 Revised Editorial no technical change A. Cockman 2000 04 17 Editorial no technical change A. Cockman 1993 05 18 Printed copies are uncontrolled Page 1 of 5 Copyright 2001, Ford Global Technologies, Inc. QUANTITATIVE ANALYSIS OF

2、TRIMETHYLAMINE Application This test method is used to determine the amount of trimethylamine found in fiberglass. Apparatus Required Glass Jar 1 liter glass with ring cap. Sink Matting Plastic Nalgene Bottles 125 mL Volumetric Flasks 50 mL 100 mL Pipets Volumetric as required. Oven Forced Air. Anal

3、ytical Balance Gas Chromatograph Split/Splitless injector and nitrogen/phosphorus or flame ionization detector. CG Column Supelcowax 10, 30 m or equivalent column for the analysis of aqueous amine samples. Vials, Septum-Sealed FORD LABORATORY TEST METHOD AO 107-01 Page 2 of 5 Copyright 2001, Ford Gl

4、obal Technologies, Inc. Materials Required Sodium Hydroxide 2 M aqueous solution. Trimethylamine Hydrochloride Water Distilled deionized, freshly boiled. Polyethylene Film Conditioning and Test Conditions All test values indicated herein are based on material conditioned in a controlled atmosphere o

5、f 23 +/- 2 C and 50 +/- 5 % relative humidity for not less than 24 h prior to testing and tested under the same conditions unless otherwise specified. Procedure I. Preparation of Trimethylamine (TMA) Stock Solution and Standards 1. Accurately weigh 0.1617 g trimethylamine hydrochloride into a 100 mL

6、 volumetric flask and dilute to volume with freshly boiled distilled, deionized water to give a 1000 ppm TMA stock solution. 2. Pipet stock solution into 50 mL volumetric flasks as described below: mL of Stock ppm TMA standard 5.0 100 2.0 40 1.0 20 0.5 (500 microliter) 10 0.2 (200 microliter) 4 0.05

7、 (50 microliter) 1 3. Dilute to volume with freshly boiled distilled, deionized water. 4. Prepare working standards by pipeting 1.71 mL of each standard solution into septum-sealed vials. Add 90 microliter of 2 M sodium hydroxide to each and mix. FORD LABORATORY TEST METHOD AO 107-01 Page 3 of 5 Cop

8、yright 2001, Ford Global Technologies, Inc. II. Sample Preparation 1. Cut samples into 25 millimetre cubes and mix thoroughly. 2. Pipet 10.0 mL boiled distilled water into a glass liter jar. 3. Place a 6.5 cm tall sample support (open-ended 125 mL nalgene bottle with end cut off) in the jar, and bal

9、ance an 8.9 cm diameter disk of sink matting upon the sample support. 4. Place 10 +/- 0.05 g of sample on the sink matting, cover the jars with polyethylene film, and screw the lids on securely. 5. Place the jars in an oven at 65 C for 16 h. 6. Remove the jars from the oven and allow to cool to 23 +

10、/- 2 C for 30 minutes. 7. Transfer 1.71 mL of test water from the jar to a septum-sealed vial. 8. Add 90 microliter of 2 M NaOH to the vial. III. Gas Chromatographic Analysis of Standards and Samples 1. Gas chromatographic conditions are as follows: Column: Supelcowax-10, 30 m or equivalent 40 C for

11、 3 min, then to 150 C 10 C/min Injector: Split/Splitless 10:1 split ratio minimum 220 C Detector: Phosphorus-Nitrogen or Flame Ionization (See Note 1) 220 C Injection: 1 microliter FORD LABORATORY TEST METHOD AO 107-01 Page 4 of 5 Copyright 2001, Ford Global Technologies, Inc. 2. A linear calibratio

12、n curve is prepared by analyzing the working standards. The TMA elutes at approximately 3.5 minutes. Peak area vs. concentration is fitted to a linear calibration curve. 3. The samples are analyzed in the same manner. The TMA content is determined using the established calibration curve. Results are

13、 reported as parts per million TMA in fiberglass. Chemicals, materials, parts, and equipment referenced in this document must be used and handled properly. Each party is responsible for determining proper use and handling in its facilities. FORD LABORATORY TEST METHOD AO 107-01 Page 5 of 5 Copyright 2001, Ford Global Technologies, Inc. QUANTITATIVE ANALYSIS OF TRIMETHYLAMINE Trimethylamine Test Set-up

展开阅读全文
相关资源
猜你喜欢
  • ASTM A928 A928M-2013 Standard Specification for Ferritic Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal《具有填充金属的铁素体 奥氏体(双相)不锈钢管电熔焊的标准规.pdf ASTM A928 A928M-2013 Standard Specification for Ferritic Austenitic (Duplex) Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal《具有填充金属的铁素体 奥氏体(双相)不锈钢管电熔焊的标准规.pdf
  • ASTM A928 A928M-2014 Standard Specification for Ferritic Austenitic &40 Duplex&41 Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal《具有填充金属的铁素体 奥氏体 (双相) 不锈钢管.pdf ASTM A928 A928M-2014 Standard Specification for Ferritic Austenitic &40 Duplex&41 Stainless Steel Pipe Electric Fusion Welded with Addition of Filler Metal《具有填充金属的铁素体 奥氏体 (双相) 不锈钢管.pdf
  • ASTM A929 A929M-2001(2007) Standard Specification for Steel Sheet Metallic-Coated by the Hot-Dip Process for Corrugated Steel Pipe《波纹钢管用的经热浸处理的金属涂覆薄钢板的标准规范》.pdf ASTM A929 A929M-2001(2007) Standard Specification for Steel Sheet Metallic-Coated by the Hot-Dip Process for Corrugated Steel Pipe《波纹钢管用的经热浸处理的金属涂覆薄钢板的标准规范》.pdf
  • ASTM A929 A929M-2001(2013) Standard Specification for Steel Sheet Metallic-Coated by the Hot-Dip Process for Corrugated Steel Pipe《波纹钢管用经热浸处理的金属涂覆薄钢板标准规格》.pdf ASTM A929 A929M-2001(2013) Standard Specification for Steel Sheet Metallic-Coated by the Hot-Dip Process for Corrugated Steel Pipe《波纹钢管用经热浸处理的金属涂覆薄钢板标准规格》.pdf
  • ASTM A929 A929M-2017 Standard Specification for Steel Sheet Metallic-Coated by the Hot-Dip Process for Corrugated Steel Pipe《用于波纹钢管的热浸镀工艺的金属涂覆钢板的标准规格》.pdf ASTM A929 A929M-2017 Standard Specification for Steel Sheet Metallic-Coated by the Hot-Dip Process for Corrugated Steel Pipe《用于波纹钢管的热浸镀工艺的金属涂覆钢板的标准规格》.pdf
  • ASTM A929 A929M-2018 Standard Specification for Steel Sheet Metallic-Coated by the Hot-Dip Process for Corrugated Steel Pipe.pdf ASTM A929 A929M-2018 Standard Specification for Steel Sheet Metallic-Coated by the Hot-Dip Process for Corrugated Steel Pipe.pdf
  • ASTM A930-2003 Standard Practice for Life-Cycle Cost Analysis of Corrugated Metal Pipe Used for Culverts Storm Sewers and Other Buried Conduits《涵洞、雨水管道和其它地下管道用波纹形金属管寿命周期成本分析的标准实施.pdf ASTM A930-2003 Standard Practice for Life-Cycle Cost Analysis of Corrugated Metal Pipe Used for Culverts Storm Sewers and Other Buried Conduits《涵洞、雨水管道和其它地下管道用波纹形金属管寿命周期成本分析的标准实施.pdf
  • ASTM A930-2009 Standard Practice for Life-Cycle Cost Analysis of Corrugated Metal Pipe Used for Culverts Storm Sewers and Other Buried Conduits《涵洞、雨水管道和其它地下管道用波纹形金属管寿命周期成本分析的标准实施.pdf ASTM A930-2009 Standard Practice for Life-Cycle Cost Analysis of Corrugated Metal Pipe Used for Culverts Storm Sewers and Other Buried Conduits《涵洞、雨水管道和其它地下管道用波纹形金属管寿命周期成本分析的标准实施.pdf
  • ASTM A930-2009(2014) Standard Practice for Life-Cycle Cost Analysis of Corrugated Metal Pipe Used for Culverts Storm Sewers and Other Buried Conduits《涵洞 暴雨下水道和其它地下的排水道用波形金属管的寿命周期费用.pdf ASTM A930-2009(2014) Standard Practice for Life-Cycle Cost Analysis of Corrugated Metal Pipe Used for Culverts Storm Sewers and Other Buried Conduits《涵洞 暴雨下水道和其它地下的排水道用波形金属管的寿命周期费用.pdf
  • 相关搜索

    当前位置:首页 > 标准规范 > 国际标准 > 其他

    copyright@ 2008-2019 麦多课文库(www.mydoc123.com)网站版权所有
    备案/许可证编号:苏ICP备17064731号-1