1、FORD LABORATORY TEST METHOD BN 027-01 2001 0823 ADHESIVE WEIGHT TEST FOR LANDAU ROOFS Revised Editorial - no technical change A. Cockman Application This procedure is used to determine the weight in ounces per square yard of adhesive sprayed on Landau roofs. Apparatus Required La bo ratory Balance A
2、ccurate to 0.1 mg. Aluminum Foil Household type, Reynolds, or equivalent. Double Backed Adhesive Tape Arno Tape, Michigan City, Indiana, or equivalent. Oven Convection type. Conditioning and Test Conditions All test values indicated herein are based on material conditioned in a controlled atmosphere
3、 of 23 +/- 2 OC and 50 +/- 5 % relative humidity for not less than 24 h prior to testing and tested under the same conditions unless otherwise specified. Procedure 1. 2. Weigh the foil sections. Cut three 4 by 4 inch sections from a roll of foil. 3. Place foil adjacent to, or directly on, the substr
4、ate to be sprayed, in a random arrangement to obtain values representative of the entire surface being sprayed. Note: Foil may be secured to test surface with double backed tape. I Date I Action I Revisions I Copynght02001, Ford Global Technologies, Inc FORD LABORATORY TEST METHOD BN 027-01 4. Follo
5、wing application of adhesive, remove foil and place them in a convection oven at 180 OF for four hours. Note: Remove the tape from the foil. 5. After removal from oven, weigh foil and calculate weight in ozlsq yd. Report the average of three weights. 6. Calculate as follows: W2 - W1 = W3 (W3) . (2.8
6、6) = x Where: W2 = Weight in grams of foil and adhesive/l6 sq. in. section W1 = Weight in grams of foil/l6 sq. in. section W3 = Weight in grams of adhesive/l6 sq. in. section X = weight of adhesive in ozlsq yd. Chemicals, materials, parts, and equipment referenced in this document must be used and handled properly. Each party is responsible for determining proper use and handling in its facilities. Page 2 of 2 Copynght02001, Ford Global Technologies, Inc