SAE AMS 2362C-2007 Stress-Rupture Properties of Castings《铸件的应力断裂特性》.pdf

上传人:lawfemale396 文档编号:1020562 上传时间:2019-03-21 格式:PDF 页数:3 大小:240.67KB
下载 相关 举报
SAE AMS 2362C-2007 Stress-Rupture Properties of Castings《铸件的应力断裂特性》.pdf_第1页
第1页 / 共3页
SAE AMS 2362C-2007 Stress-Rupture Properties of Castings《铸件的应力断裂特性》.pdf_第2页
第2页 / 共3页
SAE AMS 2362C-2007 Stress-Rupture Properties of Castings《铸件的应力断裂特性》.pdf_第3页
第3页 / 共3页
亲,该文档总共3页,全部预览完了,如果喜欢就下载吧!
资源描述

1、_SAE Technical Standards Board Rules provide that: “This report is published by SAE to advance the state of technical and engineering sciences. The use of this report isentirely voluntary, and its applicability and suitability for any particular use, including any patent infringement arising therefr

2、om, is the sole responsibility of the user.”SAE reviews each technical report at least every five years at which time it may be reaffirmed, revised, or cancelled. SAE invites your written comments and suggestions.Copyright 2012 SAE InternationalAll rights reserved. No part of this publication may be

3、 reproduced, stored in a retrieval system or transmitted, in any form or by any means, electronic, mechanical, photocopying, recording, or otherwise, without the prior written permission of SAE.TO PLACE A DOCUMENT ORDER: Tel: 877-606-7323 (inside USA and Canada)Tel: +1 724-776-4970 (outside USA)Fax:

4、 724-776-0790Email: CustomerServicesae.orgSAE WEB ADDRESS: http:/www.sae.orgSAE values your input. To provide feedbackon this Technical Report, please visithttp:/www.sae.org/technical/standards/AMS2362CAEROSPACEMATERIALSPECIFICATIONAMS2362 REV. CIssued 1966-09Revised 2007-07Reaffirmed 2012-10Superseding AMS2362BStress-Rupture Properties of CastingsRATIONALEAMS2362C has been reaffirmed to comply with the SAE five-year review policy.SAE AMS2362C Page 2 of 3SAE AMS2362C Page 3 of 3